    Good job Vince, and you're right on about the cold saw...I can't imagine going back and using the abrasive saw again, after my Makita 1230.

    Leave a comment:


  • cope
    replied
    Looks good. Flux core is the way to go with galvanized. Looks like you "had to buy" some new clamps, you can never have too many clamps.

    Leave a comment:


  • ArtisanFarms
    replied
    I always grind off the galvanized before I weld, be safe.

    Leave a comment:


  • Wheat
    replied
    Looks good!!! Only as a reminder for everybody, be careful when welding galvanized. It will definitley make you sick if inhaled.

    Leave a comment:


  • IamVince
    started a topic The Hand rail

    The Hand rail

    I'm using a Lincoln 180 set at a and 1.5. Using fluxcore (outside) .035 Welding very thin galvanized stock (16 ga or 1/16" )
    This is my first hand rail and there is not any shake in it.The welds are not as nice as I've seen on here but with stuff that thin I am sure I got plenty of penetration.
    Plum and straight right?






    I should finish up in the morning...not too bad for a couple of cabinet guys.
    I did ask my boss if there was enough left over in the budget to get me a drycut saw...Told me to look on ebay and get one.
    Last edited by IamVince; 01-06-2009, 02:32 PM.