    HELP ANYONE


    I just got an old linde VI 400 had it all went through it all worked great at the repair shop it can be set to 460/230V 3 phaze i had told the repair man we have 230V 3 phaze we hooked this welder up at home and it dosent work so we are gussing it is set up for 460V how do we switch to 230V on this welder or how can we get ahold of a owners mannual the repair man is now on vacation till jan.11 so i hope for som help so i dont have to wait till he comes back



    THANK YOU FOR ANY AND ALL HELP!!!

    MN_MI

  • #2
    Residental areas are only 1 phase unless someone paid to have 3 phase power.

    Comment


    • #3
      mn-mi,

      Unless you live in an industrial section, it's highly unlikely that you have 3 ph power installed in your home.

      What makes you think you've got 3 ph power?

      Don't think that unit can be converted to operate on 1 ph current.
      SundownIII

      Syncrowave 250DX, Tigrunner
      Dynasty 200 DX w/CM 3
      MM 251 w/30 A SG
      HH 187 Mig
      XMT 304 w/714D Feeder & Optima Pulser
      Dialarc 250 w/HF 15-1
      Hypertherm PM 1250 Plasma
      Victor, Harris, and Smith O/A
      PC Dry Cut Saw and (just added) Wilton (7x12) BS
      Mil Mod 6370-21 Metal Cut Saw
      More grinders than hands (Makita & Dewalt)
      Grizzly 6"x48" Belt Sander
      Access to full fab shop w/CNC Plasma & Waterjet
      Gas mixers (Smith(2) and Thermco)
      Miller BWE and BWE Dig

      Comment


      • #4
        ...another "Bargain" on an industrial machine, perhaps???
        "Good Enough Never Is"

        Comment


        • #5
          I would like to run into one of these 3 phase bargains. My shop is 3 ph but I would like something I could load on my truck and bring to a customers. None of my customers have 230v single phase in the shops its all 575 3ph. Either that or a deal on a nice SA-200 on a trailer would be sweet.

          Comment


          • #6
            we do have 230 3 phaze in our shop

            we do have 230 3 phaze in our shop
            Originally posted by mn-mi View Post
            HELP ANYONE


            I just got an old linde VI 400 had it all went through it all worked great at the repair shop it can be set to 460/230V 3 phaze i had told the repair man we have 230V 3 phaze we hooked this welder up at home and it dosent work so we are gussing it is set up for 460V how do we switch to 230V on this welder or how can we get ahold of a owners mannual the repair man is now on vacation till jan.11 so i hope for som help so i dont have to wait till he comes back



            THANK YOU FOR ANY AND ALL HELP!!!

            MN_MI

            Comment


            • #7
              owners info

              I have the voltage change over info but don't know how to attach it to this form. I could send it via E-mail?
              O.F.

              Comment


              • #8
                OF, I can more than likely host the file and post it here so it's of a legible size - that way it's available to others who may come searching the topic at a later date.
                Zrexxer
                Senior Member
                Last edited by Zrexxer; 01-02-2009, 10:49 AM.
                Trailblazer 302 * Millermatic 212 * Syncrowave 180SD * X-Treme 12VS Feeder * Spoolmate 3035
                Thermal Dynamics Cutmaster 52 Plasma * Lincoln 175 MIG

                Victor Superrange II * Victor Journeyman

                Hobart HH 125EZ


                Comment


                • #9
                  OK, see how this looks. It should be legible.

                  Trailblazer 302 * Millermatic 212 * Syncrowave 180SD * X-Treme 12VS Feeder * Spoolmate 3035
                  Thermal Dynamics Cutmaster 52 Plasma * Lincoln 175 MIG

                  Victor Superrange II * Victor Journeyman

                  Hobart HH 125EZ


                  Comment

                  Working...
                  X