  • Mig welding with straight CO2

    Using straight CO2, and .030 steel wire, what is the recommended setting for CO2 gas flow at the flowmeter?

  • #2
    Around 20 cfh.

    Depending on the environment (mainly wind/drafts), you can get away with a little less, or might need a little more.

    Comment


    • #3
      Most manufacture list this and other information on there web sites