  • what size wire should i use

    i have a hh140 would i get better penitration with .030 or .023 whe welding
    1/8 material

  • #2
    For 1/8" material, you will do good with .030" wire.

    Comment


    • #3
      I like the .030 on most any projects.
      Capitol Punishment

      Comment


      • #4
        thanks for the reply