Hello.
We have a Champion 145 Welder. We were using it, took a break, and then fired it back up. We had no arc and no power at receptacles. We can see the rotor and stator spinning but have no power. We're not sure if it's brushes or rectifier, not sure how to check if it's the rectifier.
How would we check if the rectifier is the problem?
Thank you!
Becky
We have a Champion 145 Welder. We were using it, took a break, and then fired it back up. We had no arc and no power at receptacles. We can see the rotor and stator spinning but have no power. We're not sure if it's brushes or rectifier, not sure how to check if it's the rectifier.
How would we check if the rectifier is the problem?
Thank you!
Becky