    how you doing, i have a hobart GF-250 welder, with the ford 200 in-line six , serial #10-4W-1756, 5517B i had it for well over 20 years with out any problems other then engine turn ups and points adjustments,. i was welding some brackets on my dozer for a root rake and it stop welding.im getting 110 volt to the plug to run a grinder but it will not strike an arc. is there anyone on here that has worked on a machine like this. thanks