Announcement

Collapse
No announcement yet.

Ranger 8, no output.

Collapse
X
 
  • Filter
  • Time
  • Show
Clear All
new posts

  • Ranger 8, no output.

    A friend asked if I would look at, being as I have a ranger 8 myself figured we could test his parts on my machine. My trouble shooting guide makes reference #216 (12v) at the board to ground. This machine does not have a #216 lead? I don't believe the generator is being excited ??? Help

  • #2
    When did it last work, or was it acquired in this condition?

    Is there a more specific model number? They've been making the Ranger 8 for so long they are probably several generations, but I don't know. There will be some guys here that may need to know in order to help.

    What troubleshooting manual are you using? Does YOUR machine have the #216 lead?

    Engine starts and runs/idles well?