  • Champion 10000 welder won’t turn off

    Hobart champion 10000 welder welds great and generator makes power but when the key is turned off unit still running already replaced the ignition switch

  • #2
    If it's like a lot of welders...……...it probably has a shut down solenoid. Generally, on a Kohler at least, they're at the base of the carb. Look for wires going to the carb,, then tap the solenoid to see if it shuts down. If so...….replace the solenoid. GET READY FOR STICKER SHOCK!!!!!!!! Those suckers run about $100

    Comment


    • #3
      Originally posted by farmersamm View Post
      If it's like a lot of welders...……...it probably has a shut down solenoid. Generally, on a Kohler at least, they're at the base of the carb. Look for wires going to the carb,, then tap the solenoid to see if it shuts down. If so...….replace the solenoid. GET READY FOR STICKER SHOCK!!!!!!!! Those suckers run about $100
      This may show what the poster above is talking about:

      Click image for larger version

Name:	Screen Shot 2020-02-12 at 3.28.05 PM.png
Views:	19
Size:	251.8 KB
ID:	707872

      Comment

      Working...
      X