When i turn it on it blows the 50 amp breaker at panel. Everything was working great, i stopped welding and a hour later i turned it off at lunch. when i turned it on after lunch it blew the breaker. I thought it was the transformer and replaced it but the same thing happened. Model #kf819114. Fuses are ok, power switch seems ok, it did not overheat. What am i missing?