Announcement

Collapse
No announcement yet.

Will .023/.024 Wire Help Me Make a Smaller Bead?

Collapse
X
 
  • Filter
  • Time
  • Show
Clear All
new posts

  • Will .023/.024 Wire Help Me Make a Smaller Bead?

    I am going to be welding some small mild steel brackets with my HH175 and want to make the bead size as small as possible without compromising penetration. I normally use .030 wire.

    Just wondering whether using .023/.024 wire will give me a little more control over making the bead smaller without hurting weld quality?

    Thanks

  • #2
    Smaller wire will help some.