    I passed my first bend test! No cracks or any weld defects, just a nice, perfect bend. I'm very pleased.

    The specimen in the picture was taken from a coupon of 1" plate that I welded as an open root V butt in the 2G position. The root pass was done with 6010, and then the hot pass and the filler was done with 7018. The root pass was gouged out with air-carbon arc and then welded back in with 7018.

    3 specimens were taken from the coupon, they all passed.
    Lincoln Idealarc 250
    Lincoln Weldanpower CC/CV engine drive
    Lincoln LN-25 wire feeder
    Miller Syncrowave 180 SD
    Various oxy-fuel setups featuring Victor, Harris, and Prest-o-lite products

  • #2
    Just aint nothing like a good clean bend.

    Congrates.

    Jim
    IN GOD WE TRUST!

    If you can't dazzle them with brilliance, Baffle them with bull$***.

    AMERICA-LOVE IT OR LEAVE IT!

    Comment


    • #3
      As a instructor...Nothing makes me happier than seeing good test piece!!
      Jonesy

      Comment


      • #4
        This past week I finally got around to bend testing some of my 3G and 4G 7018 open root butt plates and they passed too.
        Lincoln Idealarc 250
        Lincoln Weldanpower CC/CV engine drive
        Lincoln LN-25 wire feeder
        Miller Syncrowave 180 SD