It does appear to be TIG wire, but if the ID is gone, there is no way of knowing what it is. Some wires have the ID stamped on them in tiny letters, or have a color coded paint on one end.
K & S Engineering
6917 West 59th Street, Chicago, IL 60638
map | driving directions
phone: (773) 586-8503
Millermatic Passport Plus
Millermatic 200 Millermatic 350P with Python XMT 304 /w S-64 feeder and 12RC Dynasty 300 DX
Victor O/A
Premier Power Welder for my trail junk.
Like the others said, sounds like piano wire. To be sure put on a pair of safety glasses, take two pliers, grab the wire with both leaving about a 1/4" space between them. Now try to bend the wire quickly. If it snaps in half its definitely piano wire. Uncrichie.