    Hello,
    I have quite a bit of exhaust pipe that I cut up thinking it would be good to practice welding thin tubing with. It came from summit racing and there ad for it says it's Aluminized. It kinda looks like it Galvenized. Does anybody know if this stuff has the same dangers as Galvinized? It seems like it comes off real easy with the wire wheel. Any input would be great.
    Thanks

  • #2
    Aluminized exhaust has an aluminum coating instead of zinc, probably because exhaust gets hot. Since it's not zinc, so it does not pose the same danger. I wouldn't go out of my way to sniff the welding fumes though.

    Dave
    Still building my new old truck - see the progress!
    http://www.ford-trucks.com/forums/65...-coe-idea.html
    http://www.hobartwelders.com/weldtal...ad.php?t=27017

    Square Wave TIG 200 - Woot!
    MM180
    SP125+

    Comment


    • #3
      Thanks for the reply Dave. Thats what I was kinda thinking but wasnt sure.

      Comment


      • #4
        You might also see this thread, in case you are wondering about welding it.

        http://www.hobartwelders.com/weldtal...luminized+pipe
        Lincoln 175HD
        Miller Thunderbolt AC/DC
        Smith AW1, Dillon (Henrob) Mark III & Smith Quickbraze Little Torch

        Comment


        • #5
          Article about Bloxide:

          http://www.safetyonline.com/content/...&VNETCOOKIE=NO
          --- RJL ----------------------------------------------

          Ordinarily I'm insane, but I have lucid moments when I'm merely stupid.
          -------------------------

          Comment


          • #6
            smyrna5, Thanks for the link. I guess I should of used the search button

            usmcpop, That sound like the stuff we used at the bodyshop I worked at years ago, but I think the only thing it said on the can was " weldable primer "