    With stainless my rule of thumb is use the smallest tungsten and filler rod for the most cosmetic welds.....Within reason of course..I like 1/16 tungsten and .030 filler on small parts (like the one illustrated) I grind my tungsten's with a long slow taper
    and not pointed on the end just kinda blunt....Sharp but not needle sharp....
    I like gas lens with medium cups....

    Leave a comment:


  • 81Malibu
    replied
    I wish we'd get more stuff like that. I love TIG'in on new stainless. What kind of grind/taper do you like on your tungsten? How many amps, size of filler/tung. etc etc.. I like to hear what all the good TIG welders like to use to try and better myself...Cheers!

    Leave a comment: