    hi guys just a few pics of some tig 6" carbon sch 40 .the set uo is 4mm gap and fether edge prep,125-130 amp root...175amp fill and cap
    THE IMPOSIBLE I CAN DO,MIRACLES TAKE A LITTLE LONGER

  • #2
    Looks good you're hired.
    sigpic

    Comment


    • #3
      Nice work, hop a boat and we have plenty of work for you
      "Weld It And You Won't Be Screwed"
      Rescued from the boneyard SA-250 on a fully equipt trailer (My Wife's Explorer cries every time I hitch up)
      Trailblazer 301G (can't touch the SA-200 for stick)
      Arcair K-4000 A.K.A "The Hissing Cobra"
      HF- 251 TIG box for the TB with a Weldcrap torch, Yes I weld aluminum
      More than a toolbox full of stuff on an F-350 that is way to small

      Comment


      • #4
        cheers guys,if i had the money id be very tempted to jump a boat,work over my way is very quiet at the moment,been like this for couple of years realy..

        jay
        THE IMPOSIBLE I CAN DO,MIRACLES TAKE A LITTLE LONGER

        Comment


        • #5
          You gotta love weld candy.....
          So little time...So many machine tools.........
          www.flipmeisters.com

          Miller, Hobart & Lincoln TIG/MIG/-
          Hypertherm Plasma (Thanks Jim)
          Plasma-Cam DHC (coming shortly)
          Harris OA
          Too many motorcycles.............-
          sigpic

          Comment


          • #6
            Looks very good, I'm not used to seeing those big weaves. Wish I could do it, my job requires us to show 2 beads on the reinforcement

            Comment

            Working...
            X