I got an order for this basket today from a near by city corp yard supervisor....Their using it to retrieve debris from a sewer sump. I will weld the pole to it tomorrow. This is the same guys that I made the scrapper for earlier this year
Well it figures....Whenever I am happy with a project it comes back......The engineer that designed this basket didn't do his homework and it's too big for what they had planned on using it for.....
So now they want me to cut it up and change it ........I told them sorry guys I'll make you another one...But I don't want to mess around with cutting and changing this one (too much of a hassle).....I cam make a NEW basket faster
than cutting this one up and changing it ......