One of my projects today, made from 12" 6061 channel, with holes drilled and clips welded on.
http://i94.photobucket.com/albums/l1...rkStuff017.jpg
http://i94.photobucket.com/albums/l1...rkStuff021.jpg
Pile of cut parts
http://i94.photobucket.com/albums/l1...rkStuff014.jpg
I TIGged the clips on(and everything else), the end cap was done with a spoolgun (I didn't start this job)
http://i94.photobucket.com/albums/l1...rkStuff015.jpg
http://i94.photobucket.com/albums/l1...rkStuff016.jpg
Almost done, I have 2 more tomorrow.
http://i94.photobucket.com/albums/l1...rkStuff017.jpg
http://i94.photobucket.com/albums/l1...rkStuff021.jpg
Pile of cut parts
http://i94.photobucket.com/albums/l1...rkStuff014.jpg
I TIGged the clips on(and everything else), the end cap was done with a spoolgun (I didn't start this job)
http://i94.photobucket.com/albums/l1...rkStuff015.jpg
http://i94.photobucket.com/albums/l1...rkStuff016.jpg
Almost done, I have 2 more tomorrow.
Comment